خواص مکانیکی
Rockwell Hardness۹۴Sterrad Processed; ASTM D785
Tensile Stress at yield-MD۷۸٫۶Sterrad Processed; ASTM D638MPa
Elongation at break-MD۵٫۵Sterrad Processed; ASTM D638%
Tensile modulus-MD۳٬۲۴۰Control; ASTM D638MPa
Elongation at yield۵٫۷Control; ASTM D638%
(Izod impact strength(notched۱۶٫۶Sterrad Processed; ASTM D256@Thickness 3.17 mmJ/m
Rockwell Hardness۹۴Control; ASTM D785
Tensile Stress at yield-MD۷۱٫۶۴Control;Chemical Resistance to lipids, 24hrs, 30°C; ASTM D638@Strain 1.20 %MPa
Elongation at break-MD۵٫۹Sterrad Processed; Chemical Resistance to lipids, 1.2% strain, 24hrs, 30°C+I9175; ASTM D638%
Elongation at yield۵٫۵Sterrad Processed; ASTM D638%
Tensile modulus-MD۳٬۲۶۰Sterrad Processed; ASTM D638MPa
(Izod impact strength(notched۱۹٫۲Control; ASTM D256@Thickness 3.17 mmJ/m
Tensile Stress at yield-MD۸۰٫۲۵Control; ASTM D638MPa
Elongation at break-MD۱۰٫۳Control; ASTM D638%
Tensile Stress at yield-MD۷۷٫۸۴Control;Chemical Resistance to lipids, 24hrs, 30°C; ASTM D638@Strain 1.20 %MPa
Elongation at break-MD۱۱٫۸Control;Chemical Resistance to lipids, 1.2% strain, 24hrs, 30°C; ASTM D638%