Specifications
PropertyValueUnit
Mechanical Properties
Elongation at yield5ISO 527-1/2%
(Charpy Impact Strength(unnotchedNBISO 179/1eU@Temperature 23°CkJ/m2
Strain at break-MD30ISO 527-1/2%
Charpy Impact Strength (notched)6ISO 179/1eA@Temperature -30°CkJ/m2
Tensile Stress at yield-MD96ISO 527-1/2MPa
Tensile modulus-MD3,500ISO 527-1/2MPa
(Charpy Impact Strength(unnotchedNBISO 179/1eU@Temperature -30°CkJ/m2
Charpy Impact Strength (notched)7ISO 179/1eA ، 23°CkJ/m2
Electrical Properties
Relative permittivity2.8IEC 60250@ 50 Hz
Glow WireTest825IEC 60695-2-12/13 @Thickness 2mm; GWIT°C
Comparative Tracking Index200Test solution A, CTI;IEC 60112V
Surface Resistance100,000,000,000,000IEC 60093ohm
Volume resistance1,000,000,000,000,000IEC 60093ohm-cm
Dielectric Strength16K20/P50; IEC 60243-1kV/mm
Relative permittivity2.8IEC 60250@ 1 MHz
Physical Properties
Shrinkage0.9ISO 294-4; sheet with film gate at rim, mold temperature1 80°C @Thickness 2.00 mm; in flow direction%
Melting point340تقریباISO 11357; DSC; 2nd heating°C
Melting range370 – 380during the injection molding process.°C
Density1.3ISO 1183 ، 23°Cg/mL
Shrinkage1.1ISO 294-4; sheet with film gate at rim, mold temperature1 80°C @Thickness 2.00 mm; in transverse direction%
Thermal Properties
Vicat softening temperature33510N; ISO 306°C
FlameabilityV-0IEC 60695@Thickness 3.2 mm
Thermal Expansion60Longitudinal; ISO 11359@Temperature 23.0 -55.0 °Cum/(m-°C)
Vicat softening temperature30550N; ISO 306°C
Processing Properties
MVR12ISO 1133 ، 5.0 kg,380 °CmL/10min
Mold Temperature160 – 200preferably 180°C°C