Specifications
PropertyValueUnit
Appearance Properties
Refractive index1.53ISO 489; 589nm/23°C
Physical stateگرانول
Optical Properties
Transmittance91Luminous transmittance; ISO 13468-2; D65%
Processing Properties
MVR5ISO 1133@ 260°C / 10kgmL/10min
Drying Temperature<130Predrying Temperature°C
Dry Time120 – 180Predrying Time in Desiccant-Type Driermin
Mold Temperature110Injection Molding°C
Thermal Properties
Thermal Expansion53ISO 11359@ 0 - 50°Cum/(m-°C)
Heat Deflection temperature140ISO 75; at 0.45 MPa°C
Glass transition Temperature151ISO 11357°C
Vicat softening temperature150ISO 306; B/50°C
Heat Deflection temperature132ISO 75; at 1.8 MPa°C
Mechanical Properties
Strain at break-MD3ISO 527; 5mm/min%
(Charpy Impact Strength(unnotched20ISO 179/1eU@ 23°CkJ/m2
Tensile modulus-MD4,000ISO 527; 1mm/minMPa
Tensile Stress at break-MD8ISO 527; 5mm/minMPa
Physical Properties
Density1.21ISO 1183g/mL
Melting range250 – 280°C