Specifications
PropertyValueUnit
Mechanical Properties
(Charpy Impact Strength(unnotched60ISO 179/1eU@Temperature -30.0 °CkJ/m2
Charpy Impact Strength (notched)12ISO 179/1eA@Temperature 23.0 °CkJ/m2
Elongation at break-MD2.3ISO 527-1/2%
Tensile Stress at yield-MD140ISO 527-1/2MPa
Tensile modulus-MD11,000ISO 527-1/2MPa
Hardness Shore D84ISO 868
(Charpy Impact Strength(unnotched60ISO 179/1eU@Temperature 23.0 °CkJ/m2
Charpy Impact Strength (notched)12ISO 179/1eA@Temperature -30.0 °CkJ/m2
Electrical Properties
Dissipation Factor0.015IEC 60250@Frequency 1e+6 Hz
Comparative Tracking Index225100 drops value; IEC 60112V
Dielectric Strength31K20/P50; IEC 60243-1kV/mm
Glow WireTest960IEC 60695-2-1/0-3, @Thickness 2.00 mm°C
Volume resistance>1.00e+16IEC 60093ohm-cm
Surface Resistance10,000,000,000,000IEC 60093ohm
Dielectric Constant4.4IEC 60250@Frequency 1e+6 Hz
Physical Properties
Density1.67ISO 1183g/mL
Thermal Properties
FlameabilityV-0IEC 60695@Thickness 1.60 mm
Vicat softening temperature220Method A, 10 N; ISO 306°C
Vicat softening temperature213Method B, 50 N; ISO 306°C
FlameabilityV-0IEC 60695@Thickness 0.800 mm
Chemical Properties
Electrolytic CorrosionA1 StepIEC 60426
Processing Properties
Linear Mold Shrinkage0.002;sheet with film gate at rim, mold temperature 80°C@Thickness 2.00 mmcm/cm
Linear Mold Shrinkage0.018Transversecm/cm