Specifications
PropertyValueUnit
Electrical Properties
Dielectric Constant7IEC 60250@Frequency 100 Hz
Volume resistance1,000,000,000,000IEC 60093ohm-cm
Comparative Tracking Index200Test Solution A, 50 drops; IEC 60112V
Dissipation Factor0.033IEC 60250@Frequency 1e+6 Hz
Dielectric Strength7K20/P50; IEC 60243-1kV/mm
Dielectric Constant5IEC 60250@Frequency 1e+6 Hz
Dissipation Factor0.058IEC 60250@Frequency 100 Hz
Comparative Tracking Index175Test Solution A, 100 drops; IEC 60112V
Thermal Properties
Vicat softening temperature16050N; ISO 306°C
Heat Deflection temperature80ISO 75;at 1.8 MPa°C
FlameabilityHB@Thickness 3.20 mm
Thermal Expansion8045x15x10 mm; ISO 11359 @Temperature 23.0 -55.0 °Cum/(m-°C)
Heat Deflection temperature160ISO 75;at 0.46 MPa°C
Vicat softening temperature17510N; ISO 306°C
FlameabilityHB@Thickness 1.60 mm
Mechanical Properties
Charpy Impact Strength (notched)6ISO 179/1eA@Temperature -30.0 °CkJ/m2
Tensile modulus-MD2,800ISO 527-1/2MPa
(Charpy Impact Strength(unnotched34ISO 179/1eU@Temperature -30.0 °CkJ/m2
Tensile Stress at yield-MD45ISO 527-1/2MPa
Elongation at yield5ISO 527-1/2%
Elongation at break-MD6ISO 527-1/2%
Tensile Stress at break-MD45ISO 527-1/2MPa
Physical Properties
Density1.17ISO 1183g/mL
Melting point178Peak Temperature; ISO 3146, ISO11357°C
Moisture absorption0.5ISO 62; at Equilibrium@Temperature 23.0 °C, 50% R.H.%
Moisture absorption0.5ISO 62; at Equilibrium@Thickness 1.00 mm, 50% R.H%
Processing Properties
Linear Mold Shrinkage0.006127x12.7x3.2 mm (processing cond.acc. To ISO 1874-2)cm/cm
Linear Mold Shrinkage0.009127x12.7x3.2 mm (processing cond.acc. To ISO 1874-2); Transversecm/cm
Chemical Properties
Electrolytic CorrosionA1 StepIEC 60426
Water absorption1.2ISO 62; at Saturation@Thickness 1.00 mm%