Specifications
PropertyValueUnit
Physical Properties
Crystallization temperature285Recrystallization temperature; ISO 11357; DSC°C
Density1.3ISO 1183@ Temperature 23°Cg/mL
Melting point340ISO 11357; DSC; 2nd heating°C
Moisture absorption0.12ISO 62@ Temperature 23°C ; 50% r.h.%
Processing Properties
MVR7ISO 1133 @Load 5.0 kg,Temperature 380 °CmL/10min
Thermal Properties
Vicat softening temperature33510N; ISO 306°C
Heat Deflection temperature205ISO 75-1/2;at 0.45 MPa°C
Glass transition Temperature1452nd heating, onset; ISO 11357; DSC°C
Vicat softening temperature30550N; ISO 306°C
Heat Deflection temperature150ISO 75-1/2;at 1.8 MPa°C
Glass transition Temperature1552nd heating, midpoint; ISO 11357; DSC°C
Mechanical Properties
Elongation at yield523°C/ 50% r.h.;ISO 527-1/2%
Tensile modulus-MD3,400ISO 527-1/2MPa
Strain at break-MD>4023°C/ 50% r.h.;ISO 527-1/2%
Tensile Stress at yield-MD9523°C/ 50% r.h.;ISO 527-1/2MPa
Tensile Stress at break-MD>7023°C/ 50% r.h.;ISO 527-1/2MPa
(Charpy Impact Strength(unnotchedNBISO 179/1eU @ Temperature 23°C ; 50% r.h.kJ/m2
Charpy Impact Strength (notched)9ISO 179/1eA@ Temperature 23°C ; 50% r.h.
Chemical Properties
Water absorption0.4ISO 62;at saturation%