PropertyValueUnit
Electrical Properties
Dielectric Strength16IEC 60243-1;K20/P50kV/mm
Relative permittivity2.8IEC 60250;at 50Hz
Volume resistance1,000,000,000,000,000IEC 60093ohm-cm
Surface Resistance100,000,000,000,000IEC 60093ohm
Comparative Tracking Index200Test Solution A CTI; IEC 60112V
Glow WireTest960IEC 60695-2-12/13 @Thickness 2mm; GWFI°C
Comparative Tracking Index175100 drops value; IEC 60112V
Relative permittivity2.8IEC 60250;at 1 MHz
Glow WireTest800IEC 60695-2-12/13 @Thickness 2mm; GWIT°C
Physical Properties
Density1.3ISO 1183@ Temperature 23°Cg/mL
Melting point340 تقریباISO 11357; DSC; 2nd heating°C
Shrinkage1.1ISO 294-4; sheet with film gate at rim, mold temperature1 80°C @Thickness 2.00 mm; in transverse direction%
Melting range360 – 380during the injection molding process°C
Shrinkage0.9ISO 294-4; sheet with film gate at rim, mold temperature1 80°C @Thickness 2.00 mm; in flow direction%
Thermal Properties
Vicat softening temperature33510N; ISO 306°C
FlameabilityV-0IEC 60695@Thickness 3.2 mm
Thermal Expansion60ISO 11359 @Temperature 23.0 -55.0 °Cum/(m-°C)
Vicat softening temperature30550N; ISO 306°C
Mechanical Properties
(Charpy Impact Strength(unnotchedNBISO 179/1eU@Temperature -30°CkJ/m2
Charpy Impact Strength (notched)6ISO 179/1eA@Temperature 23°CkJ/m2
Tensile modulus-MD3,600ISO 527-1/2MPa
Strain at break-MD25ISO 527-1/2%
Tensile Stress at yield-MD98ISO 527-1/2MPa
Elongation at yield5ISO 527-1/2%
(Charpy Impact Strength(unnotchedNBISO 179/1eU@Temperature 23°C
Processing Properties
MVR20ISO 1133 @Load 5.0 kg,Temperature 380 °CmL/10min
Mold Temperature160 – 200preferably 180°C°C