Specifications
PropertyValueUnit
Thermal Properties
Heat Deflection temperature340ISO 75-1/2;at 0.45 MPa°C
Thermal Expansion10Longitudinal; ISO 11359@Temperature 23.0 -55.0 °Cum/(m-°C)
Vicat softening temperature34050N; ISO 306°C
FlameabilityV-0IEC 60695@Thickness 1.60 mm
Heat Deflection temperature330ISO 75-1/2;at 1.8 MPa°C
Vicat softening temperature34310N; ISO 306°C
Mechanical Properties
(Charpy Impact Strength(unnotched45ISO 179/1eU@Temperature 23°CkJ/m2
Strain at break-MD2ISO 527-1/2%
Charpy Impact Strength (notched)9ISO 179/1eA@Temperature 23°CkJ/m2
Tensile strength240ISO 527-1/2MPa
Tensile modulus-MD23,000ISO 527-1/2MPa
(Charpy Impact Strength(unnotched45ISO 179/1eU@Temperature -30°CkJ/m2
Charpy Impact Strength (notched)8ISO 179/1eA@Temperature -30°C
Electrical Properties
Surface Resistance100,000IEC 60093ohm
Volume resistance1,000,000IEC 60093ohm-cm
Glow WireTest875IEC 60695-2-12/13 @Thickness 2mm; GWIT°C
Glow WireTest960IEC 60695-2-12/13 @Thickness 2mm; GWFI°C
Physical Properties
Density1.38ISO 1183@Temperature 23°Cg/mL
Shrinkage0.4ISO 294-4; sheet with film gate at rim, mold temperature1 80°C @Thickness 2.00 mm; in transverse direction%
Melting range380 – 400during the injection molding process.°C
Melting point340تقریباISO 11357; DSC; 2nd heating°C
Shrinkage0ISO 294-4; sheet with film gate at rim, mold temperature1 80°C @Thickness 2.00 mm; in flow direction%
Processing Properties
Mold Temperature160 – 200preferably 180°C°C
MVR10ISO 1133 @Load 5.0 kg,Temperature 380 °CmL/10min