Mechanical Properties
Elongation at break-MD>5050 mm/min; ISO 527-1/2%
Tensile Stress at yield-MD8250 mm/min; ISO 527-1/2MPa
Charpy Impact Strength (notched)8ISO 179/1eA@Temperature -30.0 °CkJ/m2
(Charpy Impact Strength(unnotchedNBISO 179/1eU@Temperature -30.0 °CkJ/m2
Tensile modulus-MD2,200ISO 527-1/2MPa
Elongation at yield650 mm/min; ISO 527-1/2%
Hardness Shore D84ISO 868
Ball indentation Hardness130H30; ISO 2039-1MPa
Flexural strength805 mm/min, at 3.5% Strain; ISO 178MPa
Flexural modulus-MD2,700ISO 178MPa
Creep modulus2,200ISO 899-1;1hourMPa
Charpy Impact Strength (notched)9ISO 179/1eA@Temperature 23.0 °CkJ/m2
(Charpy Impact Strength(unnotchedNBISO 179/1eU@Temperature 23.0 °CkJ/m2
Elongation at yield85 mm/min, Outer fiber strain at maximum stress; ISO 178%
Flexural strength1185 mm/min; ISO 178MPa
Creep modulus800ISO 899-1;1000hoursMPa
(Charpy Impact Strength(unnotchedNBISO 179/1eU@Temperature 0.000 °CkJ/m2