Specifications
PropertyValueUnit
Processing Properties
MFI11.92380°C/5 kg- ISO 1133g/10min
Die Temperature400°C
Mold Temperature160 – 200°C
Drying Temperature160°C
Dry Time240min
Mechanical Properties
(Charpy Impact Strength(unnotchedNBISO 179/1eU, 23°CkJ/m2
Charpy Impact Strength (notched)7ISO 179/1eA, 23°C, Complete breakkJ/m2
Strain at break-MD20ISO 527-2%
Tensile Stress at yield-MD95ISO 527-1MPa
Tensile modulus-MD4,100,000MPa
(Charpy Impact Strength(unnotchedNBISO 179/1eU, -30°CkJ/m2
Charpy Impact Strength (notched)7ISO 179/1eA, -30°C, Complete breakkJ/m2
Thermal Properties
Glass transition Temperature152°C
Heat Deflection temperature155ISO 75-1, 1.8 MPa, Method A°C
FlameabilityV-0 ClassUL 94, 3.2 mm
Vicat softening temperature335ISO 306, 10N, Method A°C
Heat Deflection temperature210ISO 75-1, 0.45 MPa, Method B°C
Vicat softening temperature305ISO 306, 50N, Method B°C
Physical Properties
Density1.49ISO 1183- 23°Cg/mL
Melting point340ISO 11357, DSC - 2nd heating°C
Melting range380 – 400°C
Appearance Properties
Physical stateقرصی شکل
Chemical Properties
Water absorption0.4ISO 62, 23°C, Saturation%