Specifications
PropertyValueUnit
Electrical Properties
Volume resistance10^6×10^11IEC 60093ohm-cm
Surface Resistance10^5IEC 60093ohm
Dissipation Factor0.23%, IEC 60250, 1 MHz
Relative permittivity17IEC 60250, 1 MHz
Thermal Properties
FlameabilityV-0 ClassUL 94, 1.6 mm
Vicat softening temperature343ISO 306, 10N, Method A°C
Heat Deflection temperature330ISO 75-1, 1.8 MPa, Method A°C
Heat Deflection temperature340ISO 306, 50N, Method B°C
Vicat softening temperature34050N°C
Mechanical Properties
Charpy Impact Strength (notched)8ISO 179/1eA, -30°C, Complete breakkJ/m2
(Charpy Impact Strength(unnotched45ISO 179/1eU, 23°C, Complete breakkJ/m2
Tensile Stress at yield-MD240ISO 527-1MPa
Strain at break-MD2ISO 527-2%
Tensile modulus-MD23,000ISO 527-1/2MPa
Charpy Impact Strength (notched)9ISO 179/1eA, 23°C, Complete breakkJ/m2
(Charpy Impact Strength(unnotched45ISO 179/1eU, -30°C, Complete break
Physical Properties
Shrinkage0.4ISO 294-4, 2 mm, Transverse%
Density1.38ISO 1183- 23°Cg/mL
Melting point340ISO 11357, DSC - 2nd heating°C
Melting range380 – 400°C
Shrinkage0ISO 294-4, 2 mm, Flow%
Processing Properties
MFI13.8380°C/5 kg- ISO 1133g/10min
Mold Temperature160 – 200°C
Die Temperature390°C
Drying Temperature160°C
Dry Time240min
Appearance Properties
Physical stateقرصی شکل
Chemical Properties
Water absorption0.4ISO 62, 23°C%